Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Ryton® R10-110BL Polyphenylene Sulfide Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black Polyphenylene Sulfide CompoundRyton® R10-110BL is a glass and mineral filled polyphenylene sulfide compound which provides a good combination of mechanical and electrical properties.Applications: Insulating ComponentsComments: Test specimen molding conditions: Stock Temperature, 315-345°C; Mold Temperature, 135°C; ASTM Values Converted to SI UnitsData provided by Chevron Phillips Chemical Company LP.Solvay Specialty Polymers has acquired the Ryton product line. This product was discontinued prior to the acquisition and is listed under the Chevron Phillips name for historical purposes.
Physical Properties Metric English Comments
Density 2.05 g/cc
0.0741 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115 MPa
16700 psi
ASTM D638
Elongation at Break 0.70 %
0.70 %
ASTM D638
Flexural Yield Strength 185 MPa
26800 psi
ASTM D790
Flexural Modulus 21.0 GPa
3050 ksi
ASTM D790
Compressive Yield Strength 240 MPa
34800 psi
ASTM D695
Izod Impact, Notched 0.550 J/cm
1.03 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature 100 - 200 °C
5.00 µin/in-°F

@Temperature 212 - 392 °F
Axial; ASTM E831
13.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
7.22 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ASTM E831
CTE, linear, Transverse to Flow 24.0 µm/m-°C

@Temperature 20.0 °C
13.3 µin/in-°F

@Temperature 68.0 °F
ASTM E831
70.0 µm/m-°C

@Temperature 100 - 200 °C
38.9 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
Thermal Conductivity 0.650 W/m-K
4.51 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 220 °C
428 °F
UL Temperature Index 220 / 240 per UL746B
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Annealed 2 hr @ 200°C; ASTM D664
Flammability, UL94 5VA
5VA
UL94 V-0/5VA
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 5.00e+13 ohm

@Temperature 90.0 °C
5.00e+13 ohm

@Temperature 194 °F
95% RH, 48 hrs
Dielectric Constant 5.4

@Frequency 1e+6 Hz
5.4

@Frequency 1e+6 Hz
ASTM D150
5.5

@Frequency 1000 Hz
5.5

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mm
406 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1e+6 Hz
0.0020

@Frequency 1e+6 Hz
ASTM D150
0.0040

@Frequency 1000 Hz
0.0040

@Frequency 1000 Hz
ASTM D150
Arc Resistance 183 sec
183 sec
ASTM D495
Comparative Tracking Index 250 V
250 V
UL 746A