Material Notes:
Xtel® XE5300NA is a high performance extrusion grade PPS based alloy developed to provide excellent mechanical strength, elongation and chemical resistance.Information provided by Chevron Phillips
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527
Elongation at Yield 10 %
10 %
ISO 527
Modulus of Elasticity 2.40 GPa
348 ksi
ISO 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 315 - 345 °C
599 - 653 °F
Mold Temperature 135 °C
275 °F
Users viewing this material also viewed the following: