Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ChevronTexaco Geotex® HD SAE 40

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Geotex® HD
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Geotex® HD SAE 40.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Texaco Geotex HD is a medium ash, intermediate base number, dispersant/detergent type engine oil. It is manufactured using highly refined paraffinic base oils and an additive package containing ashless dispersant, oxidation inhibitors, metallic detergents, and a metallic antiwear agent.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 221852; MSDS Number: 8627
Physical Properties Metric English Comments
API Gravity 29.7 °
29.7 °
Viscosity Measurement 100
100
Viscosity Index
Kinematic Viscosity at 40°C (104°F) 150 cSt
150 cSt
Kinematic Viscosity at 100°C (212°F) 15 cSt
15 cSt
Ash 0.90 %
0.90 %
Sulfated Ash
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 259 °C
498 °F
Component Elements Properties Metric English Comments
Phosphorous, P 0.108 %
0.108 %
Zinc, Zn 0.12 %
0.12 %
Chemical Properties Metric English Comments
Acid Value 2.2
2.2
ASTM D 664
Total Base Number 7.6
7.6
ASTM D2896