ChevronTexaco NLGI 2 SRI Grease

Category Fluid , Lubricant , Urea Gellant
Manufacturer ChevronTexaco Corp
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco NLGI 2 SRI Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron SRI Grease is a high temperature ball and roller bearing grease.It is formulated with ISOSYN® base stocks, a synthetic polyurea ashless organic thickener, and high performance rust and oxidation inhibitors (the latter to provide superior rust protection in severe applications). Its texture is smooth and buttery and its color is dark green.Chevron SRI Grease passes ASTM D 1743 73 rust test with 5% synthetic sea water. It gives longer bearing life under high speed and high temperature operation than most other widely used antifriction bearing greases. ASTM D 3336 tests show that the life of a 204 K bearing lubricated with Chevron SRI Grease and operating at 150°C (302°F) and 10,000 rpm is about 3000 hours. This is nearly 10 times the life possible when using conventional lithium greases.ApplicationsChevron SRI Grease is recommended:for use in a wide range of automotive and industrial applicationsfor use in antifriction bearings operating at high speeds (10,000 rpm and greater)where the operating temperatures are on the order of 150°C (302°F) and higherwhere there is a likelihood that water or salt water will get into the bearingsIt performs satisfactorily in bearings at temperatures as low as -30°C (-22°F).Applications where Chevron SRI Grease will outperform most other greases include:As a "life-pack" lubricant by manufacturers of automotive generators, alternators, and starters to protect against the effects of moisture and roadsplashBearings on air-conditioning units in homes and other buildingsUnsealed electric motor bearings operating under moist conditionsApplications where silent operations are requiredOriginal Equipment Manufacturers that specifically recommend Chevron SRI Grease are:Bearing manufacturers: NSK, NTN, FAG, SKF, NMB, GMN Torrington, and American Koyo.Electric motor manufacturers: Reliance Electric Company, U.S. Motors Division of Emerson Electric Company, Toshiba International, Magnetek National Coil Company, and Lincoln Electric.Auto manufacturers: Chrysler, General Motors, and Ford.Chevron SRI Grease is registered with NSF and is acceptable as a lubricant where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.
Physical Properties Metric English Comments
Viscosity Measurement 97
97
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 606 SUS
606 SUS
Saybolt Viscosity at 210°F 69 SUS
69 SUS
Kinematic Viscosity at 40°C (104°F) 116 cSt
116 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 12.3 cSt
12.3 cSt
ASTM D445
Mechanical Properties Metric English Comments
Penetration 280
280
Worked
Penetration P(0), 1/10 mm 255
255
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Pour Point -15.0 °C
5.00 °F
ASTM D97
Flash Point 260 °C
500 °F
ASTM D92
Dropping Point 243 °C
469 °F
Descriptive Properties Value Comments
Color Dark Green
High Temperature Life, hours at 177°C, ASTM D3336 600
Lincoln Ventmeter, psig at 30 s, at 0°F 750
Lincoln Ventmeter, psig at 30 s, at 30°F 425
Lincoln Ventmeter, psig at 30 s, at 75°F 225
Texture Smooth, Buttery
Thickener, % / type 8 / Polyurea