ChevronTexaco Ulti-Plex® NLGI 0 Greases EP

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ChevronTexaco Corp
Trade Name Ulti-Plex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Ulti-Plex® NLGI 0 Greases EP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesChevron Ulti-Plex Greases EP are multipurpose, high performance greases specially formulated for extreme pressure bearing applications operating under high and low temperature conditions.They are manufactured using selected highly refined, high viscosity base oils, a lithium complex thickener, rust and oxidation inhibitors, and extreme pressure and tackiness additives. They are purple in color and stringy in texture.The lithium complex thickener in Chevron Ulti-Plex Greases EP elevates the dropping point to approximately 265°C (510°F).ApplicationsThese greases are recommended for applications operating in the temperature range of -26°C to 177°C (-15°F to 350°F). Chevron Ulti-Plex Greases EP are ideal for a wide variety of industrial and automotive applications across several industries, including:Paper and Forest Products — These lubricants are superior for severe service applications such as: sludge press bearings, lime kilns, pumps, woodyard heavy equipment, Doctor oscillator bearings, felt roll bearings, pulp refiner bearings, rope sheaves, and exhaust fan bearings.Mining — Applications appropriate for these greases include: pins and bushings on buckets and loaders, shaker screens, crushers, and conveyors.Off-Road Construction — These greases display superior water washout resistance properties in wet, off-road environments, as well as excellent shock load protection.Steel — Steel mill applications often involve extremely high temperatures. The excellent structural stability of these greases makes them appropriate in these situations. Extreme pressure properties and resistance to water washout are also key in the steel mill environment.Marine — The rust and corrosion inhibition properties of Chevron Ulti-Plex Greases EP make them ideal for use in marine equipment exposed to severe corrosion environments. Examples include deck cranes and offshore drilling equipment.
Physical Properties Metric English Comments
Viscosity Measurement 80
80
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1636 SUS
1636 SUS
Saybolt Viscosity at 210°F 106 SUS
106 SUS
Kinematic Viscosity at 40°C (104°F) 305 cSt
305 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 21 cSt
21 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Weld Point
Four Ball Wear 0.380 mm
0.0150 in
Penetration 370
370
Worked
Penetration P(0), 1/10 mm 365
365
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -26.0 °C
-14.8 °F
Flash Point 274 °C
525 °F
ASTM D92
Dropping Point 255 °C
491 °F
Descriptive Properties Value Comments
Color Purple
Corrosion, Copper Strip Test 3h 2A
Lincoln Ventmeter, psig at 30 s, at 0°F 400
Lincoln Ventmeter, psig at 30 s, at -22°F 1175
Lincoln Ventmeter, psig at 30 s, at 30°F 175
Texture Stringy
Thickener, % / type 4 / Lithium Complex