Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chi Mei Kibipol® PR-1205 Butadiene Rubber (SSBR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Chi Mei Corporation (ChiMei)
Trade Name Kibipol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chi Mei Kibipol® PR-1205 Butadiene Rubber (SSBR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Asphalt modifier
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D1646
Viscosity 10 cP
10 cP
5% Styrene Solution; ASTM D445
Mooney Viscosity 42 - 52
42 - 52
ASTM D1646
Ash <= 0.10 %
<= 0.10 %
ASTM D1646
Descriptive Properties Value Comments
Apha Color = 10
ASTM D1209
Bale Weight (Kg) 35
Butadiene/Styrene Content (%) 75/25
ASTM D1646
Cis Content (%) 35
Vinyl Content (%) 146
Wrapping Film (Type) PE
Users viewing this material also viewed the following: