Material Notes:
Product CharacteristicsWater ClearHigh RigidityMedium FlowInformation provided by Calsak Corporation
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
16 g/10 min

@Load 3.80 kg,
Temperature 230 °C
16 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 83
83
ASTM D789
Tensile Strength, Yield 60.6 MPa

@Thickness 3.17 mm
8790 psi

@Thickness 0.125 in
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 88.11 MPa

@Thickness 3.17 mm
12780 psi

@Thickness 0.125 in
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.166 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.310 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
0.176 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.330 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
unannealed; ASTM D648
100 °C
212 °F
annealed; ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.59 mm
HB

@Thickness 0.0625 in