Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer Chi Mei Corporation (ChiMei)
Trade Name Kibiton®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chi Mei Kibiton® PB-5900 Styrene-Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Injection Molding, High rigidity
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 220 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 428 °F
Melt Volume Rate (ml/10 min); ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 26.0 MPa
3770 psi
50 mm/min, 4 mm; ISO 527
Tensile Strength, Yield 40.0 MPa
5800 psi
50 mm/min, 4 mm; ISO 527
Elongation at Break 25 %
25 %
50 mm/min, 4mm; ISO 527
Elongation at Yield 2.0 %
2.0 %
50 mm/min, 4mm; ISO 527
Flexural Strength 51.0 MPa
7400 psi
2 mm/min, 4 mm; ISO 178
Flexural Modulus 2.20 GPa
319 ksi
2 mm/min, 4 mm; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched 11.0 J/cm²
52.4 ft-lb/in²
ISO 179
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
unannealed; ISO 75
83.0 °C
181 °F
annealed; ISO 75
Vicat Softening Point 76.0 °C

@Load 5.00 kg
169 °F

@Load 11.0 lb
50°C/hr; ISO 306
81.0 °C

@Load 5.00 kg
178 °F

@Load 11.0 lb
120°C/hr; ISO 306
96.0 °C

@Load 1.00 kg
205 °F

@Load 2.20 lb
50°C/hr; ISO 306
99.0 °C

@Load 1.00 kg
210 °F

@Load 2.20 lb
120°C/hr; ISO 306