Chicago Extruded Metals BioBrass® CXM10 Lead-Free Alloy

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Chicago Extruded Metals (CXM)
Trade Name BioBrass®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chicago Extruded Metals BioBrass® CXM10 Lead-Free Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Finished product available in rods.Chicago Extruded Metal temper code: H02This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals
Physical Properties Metric English Comments
Density 8.30 g/cc
0.300 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 565 - 586 MPa
82000 - 85000 psi
Tensile Strength, Yield 317 - 345 MPa
46000 - 50000 psi
Elongation at Break 30 %
30 %
Machinability 78 %
78 %
UNS C36000 (free-cutting brass) = 100%
Thermal Properties Metric English Comments
Thermal Conductivity 31.1 W/m-K
216 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 70 - 75 %
70 - 75 %
Iron, Fe 0.10 %
0.10 %
Lead, Pb 0.080 %
0.080 %
Manganese, Mn 0.080 - 1.8 %
0.080 - 1.8 %
Nickel, Ni 0.20 %
0.20 %
Other, total 0.50 %
0.50 %
Phosphorous, P 0.050 - 0.20 %
0.050 - 0.20 %
Silicon, Si 1.8 - 2.6 %
1.8 - 2.6 %
Tin, Sn 0.30 %
0.30 %
Zinc, Zn 19.22 - 26.17 %
19.22 - 26.17 %
As Balance
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000181 ohm-cm
0.0000181 ohm-cm
Users viewing this material also viewed the following: