Information provided by China Tungsten
Physical Properties Metric English Comments
Density 17.0 g/cc
0.614 lb/in³
Component Elements Properties Metric English Comments
Copper, Cu 1.0 %
1.0 %
Iron, Fe 3.0 %
3.0 %
Nickel, Ni 6.0 %
6.0 %
Tungsten, W 90 %
90 %