Good toughness, high strength, capable of resisting high impact load, Roughing of stainless steel and cast irons.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 14.6 g/cc
0.527 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 90
90
Flexural Strength 2150 MPa
312000 psi