China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics)

Category Ceramic , Oxide , Aluminum Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer China-Yixing Longly Refractories Co. Ltd
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is 1200°C. Within this temperature range, it is probably the most economical electrical insulating material commercially available. It could be used in the manufacturing of the heater bottom plate, thermocouple insulation porcelain and kiln furniture, in which high thermal shock resistance is needed. It also serves as coil skeleton, electric insulation material with arc resistance function, parent metal of compound materials, and burner nozzle of electric heating insulated device and so on.Information Provided by China Yixing Longly Refractories Co. Ltd
Physical Properties Metric English Comments
Bulk Density 2.10 - 2.30 g/cc
0.0759 - 0.0831 lb/in³
Water Absorption <= 0.0060 %
<= 0.0060 %
Mechanical Properties Metric English Comments
Hardness, Mohs 8.0
8.0
Flexural Strength >= 220 MPa
>= 31900 psi
cold bending
Compressive Strength >= 230 MPa
>= 33400 psi
Ambient
Thermal Properties Metric English Comments
CTE, linear 0.800 - 1.90 µm/m-°C

@Temperature 20.0 - 1000 °C
0.444 - 1.06 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 1.10 - 1.50 W/m-K

@Temperature 25.0 - 300 °C
7.63 - 10.4 BTU-in/hr-ft²-°F

@Temperature 77.0 - 572 °F
Maximum Service Temperature, Air >= 1200 °C
>= 2190 °F
Component Elements Properties Metric English Comments
Al2O3 60 - 80 %
60 - 80 %
Electrical Properties Metric English Comments
Volume Resistivity 1e+05 - 1.00e+6 ohm-cm

@Temperature 100 °C
1e+05 - 1.00e+6 ohm-cm

@Temperature 212 °F
>= 1.00e+15 ohm-cm

@Temperature 1000 °C
>= 1.00e+15 ohm-cm

@Temperature 1830 °F
Dielectric Strength >= 15.0 kV/mm
>= 381 kV/in
16.0 kV/mm
406 kV/in
DC Breakdown Strength
18.0 kV/mm
457 kV/in
Insulating Strength
Dielectric Loss Index 5.0 - 8.0

@Temperature 20.0 °C
5.0 - 8.0

@Temperature 68.0 °F
Descriptive Properties Value Comments
Heat-resisting Impulse T(°C) 260
MgO-SiO2 (%) 12-35
Refractoriness (°C) >1720