Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain)

Category Ceramic , Oxide , Magnesium Oxide , Silicon Oxide
Manufacturer China-Yixing Longly Refractories Co. Ltd
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good mechanical properties and electrical resistance are needed, and is one of insulating materials with relatively good strength that operates safely at temperatures up to 1200°C. It has strong acid resistance, insulation property and absorbability, and is a kind of ceramic for mounting purposes, which can be used as coil skeleton, mounting panel, bracket, various high frequency insulator, band switch porcelain axis, porcelain bushing, seal housing, resistor cores and casings and so on in the electronic products. Steatite ceramics (high frequency porcelain) has high heat insulation performance, good chemical stability, high pressure resistance and stability of electric properties with temperature and frequency variation.Information Provided by China Yixing Longly Refractories Co. Ltd
Physical Properties Metric English Comments
Bulk Density 2.80 - 3.10 g/cc
0.101 - 0.112 lb/in³
Water Absorption <= 0.00 %
<= 0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 8.5
8.5
Flexural Strength >= 280 MPa
>= 40600 psi
cold bending
Compressive Strength >= 260 MPa
>= 37700 psi
Ambient
Thermal Properties Metric English Comments
CTE, linear 6.50 - 7.10 µm/m-°C

@Temperature 20.0 - 1000 °C
3.61 - 3.94 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 2.20 - 2.50 W/m-K

@Temperature 25.0 - 300 °C
15.3 - 17.4 BTU-in/hr-ft²-°F

@Temperature 77.0 - 572 °F
Maximum Service Temperature, Air >= 1200 °C
>= 2190 °F
Component Elements Properties Metric English Comments
Al2O3 2.0 - 5.0 %
2.0 - 5.0 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 - 1.00e+9 ohm-cm

@Temperature 100 °C
1.00e+8 - 1.00e+9 ohm-cm

@Temperature 212 °F
1.00e+10 - 1.00e+12 ohm-cm

@Temperature 1000 °C
1.00e+10 - 1.00e+12 ohm-cm

@Temperature 1830 °F
Dielectric Strength >= 20.0 kV/mm
>= 508 kV/in
15.0 - 25.0 kV/mm
381 - 635 kV/in
DC Breakdown Strength
20.0 - 30.0 kV/mm
508 - 762 kV/in
Insulating Strength
Dielectric Loss Index 6.0 - 8.0

@Temperature 20.0 °C
6.0 - 8.0

@Temperature 68.0 °F
Descriptive Properties Value Comments
Heat-resisting Impulse T(°C) 200
MgO-SiO2 (%) 92-96
Refractoriness (°C) >1750