Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories CRAG-L38 Shroud Nozzle

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CRAG-L38 Shroud Nozzle.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.20 g/cc
0.0795 lb/in³
Porosity 16 %
16 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00539 - 0.00686 GPa

@Temperature 1400 °C
0.782 - 0.995 ksi

@Temperature 2550 °F
Compressive Strength 24.5 MPa
3560 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 2.00 µm/m-°C

@Temperature 1000 °C
1.11 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 41 %
41 %
SiO2 26 %
26 %
ZrO2 3.0 %
3.0 %
Descriptive Properties Value Comments
Chemical Analysis (%), FC+SiC 29+1
Remarks High spalling resistance, Corrosion resistance