Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 1.92e-7 - 0.00118 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000279 - 0.171 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0007848 - 0.0017658 GPa

@Temperature 1000 °C,
Time 10800 sec
0.1138 - 0.25611 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 1.77 - 3.43 MPa

@Temperature 1000 °C,
Time 10800 sec
256 - 498 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
2.45 - 3.92 MPa

@Temperature 110 °C,
Time 86400 sec
356 - 569 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.349 W/m-K

@Temperature 260 °C
2.42 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.3722 W/m-K

@Temperature 540 °C
2.579 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.3955 W/m-K

@Temperature 800 °C
2.740 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1200 °C
2190 °F
limited
Shrinkage -0.600 %

@Temperature 1000 °C,
Time 10800 sec
-0.600 %

@Temperature 1830 °F,
Time 3.00 hour
-0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.100 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 34 %
34 %
SiO2 47 %
47 %
Descriptive Properties Value Comments
Installation Method Gunning
Main Applications General Uses
Material Required for Estimating (kg/?) 1,300
Water Required for Casting(%) Nozzle Mixing