Chosun Refractories HM-A Special Mortar for Sliding Gate Valve

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories HM-A Special Mortar for Sliding Gate Valve.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Grain Size 75 µm
75 µm
70% <= 0.075 mm
500 µm
500 µm
1% >= 0.50 mm
Mechanical Properties Metric English Comments
Adhesive Bond Strength <= 0.981 MPa

@Temperature 110 °C,
Time 86400 sec
<= 142 psi

@Temperature 230 °F,
Time 24.0 hour
<= 2.943 MPa

@Temperature 500 °C,
Time 10800 sec
<= 426.8 psi

@Temperature 932 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 <= 68 %
<= 68 %
Descriptive Properties Value Comments
Main Applications Plate Nozzle
Material Al2O3
Refractoriness (SK) 36=