Chosun Refractories MIX-2 Light-Weight Gunning Castable

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories MIX-2 Light-Weight Gunning Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 1.44e-7 - 0.000687 GPa

@Temperature 110 °C,
Time 86400 sec
0.0000209 - 0.0996 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0004905 - 0.000981 GPa

@Temperature 1000 °C,
Time 10800 sec
0.07114 - 0.142 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 1.47 - 2.45 MPa

@Temperature 1000 °C,
Time 10800 sec
213 - 356 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
2.45 - 3.43 MPa

@Temperature 110 °C,
Time 86400 sec
356 - 498 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.174 - 0.233 W/m-K

@Temperature 540 °C
1.21 - 1.61 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.233 - 0.291 W/m-K

@Temperature 800 °C
1.61 - 2.01 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
limited
Shrinkage -1.30 - -1.00 %

@Temperature 1000 °C,
Time 10800 sec
-1.30 - -1.00 %

@Temperature 1830 °F,
Time 3.00 hour
-0.200 - -0.100 %

@Temperature 110 °C,
Time 86400 sec
-0.200 - -0.100 %

@Temperature 230 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Installation Method Gunning, Casting(UOP)
Main Applications Petrochemical plant Heater, Boiler
Material Required for Estimating (kg/?) 700-800
Water Required for Casting(%) 55