Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories SBSN-G15 Nozzle

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SBSN-G15 Nozzle.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.50 g/cc
0.0903 lb/in³
Porosity 13.5 %
13.5 %
Mechanical Properties Metric English Comments
Modulus of Rupture 0.037278 GPa

@Temperature 1400 °C
5.4068 ksi

@Temperature 2550 °F
0.03924 GPa

@Temperature 250 °C
5.691 ksi

@Temperature 482 °F
Compressive Strength 147 MPa
21300 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.00 µm/m-°C

@Temperature 1000 °C
2.22 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
SiC 80 %
80 %
Descriptive Properties Value Comments
Chemical Analysis(%),Si2ON2 15
Refractories Under Load(2kg/?,T2?) 1700<