Chosun Refractories ZR-C Special brick

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories ZR-C Special brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.55 g/cc
0.128 lb/in³
Porosity 16 %
16 %
Mechanical Properties Metric English Comments
Compressive Strength 98.1 MPa
14200 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 4.00 µm/m-°C

@Temperature 1000 °C
2.22 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
ZrO2 58 %
58 %
Descriptive Properties Value Comments
Refractories Under Load(2kg/?,T2?) 1,580
Refractoriness (SK) 36