Clariant ABS4500G10BK ABS, 10% Glass Reinforced

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant ABS4500G10BK ABS, 10% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Filler Content 12 %
12 %
ASTM D2584
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Modulus 3.90 GPa
566 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 22.8 °C
1.10 ft-lb/in

@Temperature 73.0 °F
ASTM D256