Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.66 g/cc
1.66 g/cc
ASTM D792
Filler Content 30 %
30 %
ASTM D2584
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Temperature 22.8 °C
1.20 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648
Flammability, UL94 V-0
V-0
1/32, 1/16, 1/8, 1/4
Processing Properties Metric English Comments
Rear Barrel Temperature 221 - 249 °C
430 - 480 °F
Middle Barrel Temperature 227 - 254 °C
440 - 490 °F
Front Barrel Temperature 232 - 260 °C
450 - 500 °F
Nozzle Temperature 238 - 266 °C
460 - 510 °F
Melt Temperature 232 - 260 °C
450 - 500 °F
Mold Temperature 82.2 - 121 °C
180 - 250 °F
Dry Time <= 4 hour
<= 4 hour
to ensure the moisture level is less than 0.02%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 MPa
50.0 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 25 - 100 rpm
25 - 100 rpm