Clariant PE20000FR Olefin, Flame Retardant, Non Halogen

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Clariant
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant PE20000FR Olefin, Flame Retardant, Non Halogen.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256