Clariant Renol 6601L Nylon 66, Lubricated

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol 6601L Nylon 66, Lubricated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.020 cm/cm
0.015 - 0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.8 MPa
11000 psi
ASTM D638
Elongation at Yield 50 %
50 %
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Temperature 22.8 °C
0.900 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 227 °C
440 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 271 - 293 °C
520 - 560 °F
Mold Temperature 65.6 - 79.4 °C
150 - 175 °F
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm