Clariant Renol PA2SP0006 Nylon 6, Heavyweight Compound

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PA2SP0006 Nylon 6, Heavyweight Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 5.20 g/cc
5.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.010 cm/cm
0.0050 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Flexural Modulus 9.79 GPa
1420 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Temperature 22.8 °C
1.10 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 227 - 254 °C
440 - 490 °F
Mold Temperature 79.4 - 107 °C
175 - 225 °F
Dry Time 2 - 4 hour

@Temperature 79.4 °C
2 - 4 hour

@Temperature 175 °F
to ensure moisture content is less than 0.2%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm