Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic/Polycarbonate Alloy , Polycarbonate (PC)
Manufacturer Clariant
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Flexural Yield Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 12.8 J/cm
24.0 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 238 - 266 °C
460 - 510 °F
Mold Temperature 65.6 - 98.9 °C
150 - 210 °F
Injection Pressure 33.1 - 41.4 MPa
4800 - 6000 psi
Secondary
55.2 - 68.9 MPa
8000 - 10000 psi
Initial
Back Pressure 0.345 - 2.07 MPa
50.0 - 300 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 80 - 100 rpm
80 - 100 rpm
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved