Material Notes:
Data provided by Clariant Masterbatches
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm

@Temperature 22.8 °C
0.500 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
Processing Properties Metric English Comments
Melt Temperature 182 - 210 °C
360 - 410 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Dry Time 2 - 4 hour

@Temperature 121 °C
2 - 4 hour

@Temperature 250 °F
to ensure moisture level is less than 0.2%
Injection Pressure 4.96 - 8.27 MPa
720 - 1200 psi
Secondary
8.27 - 13.8 MPa
1200 - 2000 psi
Initial
Back Pressure 0.345 - 1.72 MPa
50.0 - 250 psi
Shot Size 30 - 80 %
30 - 80 %
Screw Speed 20 - 100 rpm
20 - 100 rpm