Claude Bamberger Ultimax® 9100 Purge Compound

Category Polymer , Thermoplastic , Purging Compound
Manufacturer Claude Bamberger
Trade Name Ultimax®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Claude Bamberger Ultimax® 9100 Purge Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ultimax® is recommended for ABS, nylon, polycarbonate, PET, and other high temperature engineering plastics. Temperature range 350-525°F (176-275°C). Ultimax® 9100 is environmentally friendlier. Formulated to flow through injection cylinders and extrusion barrels without scratching. Recommended for use in swift color and resin changeover and to clean machines of carbonized residue. Ultimax® will not melt completely and are excellent for difficult purging jobs.Information provided by Claude Bamberger Molding Compounds.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 350 - 450 °C
662 - 842 °F
Cellulosics, Polyolefins, Styrenics & PVC Resins
400 - 550 °C
752 - 1020 °F
High Temperature Engineering Polymers