Colorite Polymers Vinylbond 96-1050-21 BLACK Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Colorite Polymers
Trade Name Vinylbond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Colorite Polymers Vinylbond 96-1050-21 BLACK Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Vinylbond 96-1050-21 BLACK is a flexible vinyl extrusion compound formulated specifically for the window market industry. This particular compound offers excellent bonding characteristics to ABS and PETG which makes it ideal for coextrusion applications.Information provided by Colorite Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
ASTM D2240
Tensile Strength, Ultimate 15.7 MPa
2270 psi
ASTM D638
Elongation at Break 490 %
490 %
ASTM D638
100% Modulus 0.00593 GPa
0.860 ksi
ASTM D638
Tear Strength 50.0 kN/m
285 pli
ASTM D624