ConocoPhillips 1 HD Calcium Grease NLGI No. 1

Category Fluid , Lubricant , Calcium Gellant , Organic Soap Gellant
Manufacturer ConocoPhillips
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips 1 HD Calcium Grease NLGI No. 1.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco HD Calcium Grease is a formulated product, ideally suited for equipment exposed to corrosive fluids, saltwater or extremely high temperatures. HD Calcium Grease is used exclusively by NASA in the space shuttle program due to its resistance to saltwater corrosion. Natural tackiness, water washout resistance and load-carrying ability make HD Calcium Grease useful in large, low-speed, heavily loaded industrial antifriction bearings and slow-speed open gearing. HD Calcium Grease's calcium-sulfonate thickener is a gel or “nonsoap” grease type. This provides a grease which is resistant to oil bleeding, handles high temperatures (up to 500°F (260°C), 350°F (177°C) continuous), is shear stable and is nearly impervious to water washout. Rust and corrosion protection is good, particularly over long periods since water, air and other corrosive material cannot penetrate the gel structure of the grease as easily as with soap-thickened greases.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Viscosity Measurement 95
95
Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 2177 SUS
2177 SUS
Base Oil Property
Saybolt Viscosity at 210°F 149 SUS
149 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 470 cSt
470 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 31.5 cSt
31.5 cSt
Base Oil
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 46
46
Four Ball Extreme Pressure, Weld Load 500 kg
1100 lb (mass)
Four Ball Wear 0.460 mm
0.0181 in
Penetration P(60), 1/10 mm 325
325
Timken Test 15900 g
35.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 191 °C
375 °F
Minimum Service Temperature, Air -12.2 °C
10.0 °F
Pour Point -12.2 °C
10.0 °F
(Base Oil Property)
Dropping Point 288 °C
550 °F
Descriptive Properties Value Comments
ASTM Rust Fresh and Saltwater Pass
Color Tan-Brown
Copper Corrosion 1B
Oil Separation 0 wt.%
Roll Stability 0.6% Change
Thickener Calcium Sulfonate
Water Washout 0