Material Notes:
Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures. Inca Oil is manufactured with high viscosity-index paraffinic base oils. It is compounded with an acidless tallow oil to emulsify with moisture and provide excellent wettability and lubricity to cylinder and valve surfaces in the presence of wet steam or water. It possesses film strength and oiliness characteristics, which makes it an excellent lubricant for worm gear applications.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
Viscosity Measurement 84
84
Viscosity Index
Saybolt Viscosity at 100°F 4632 SUS
4632 SUS
Saybolt Viscosity at 210°F 215 SUS
215 SUS
Kinematic Viscosity at 40°C (104°F) 1000 cSt
1000 cSt
Kinematic Viscosity at 100°C (212°F) 46 cSt
46 cSt
ASTM Color 6.5
6.5
Thermal Properties Metric English Comments
Pour Point 10.0 °C
50.0 °F
Flash Point 316 °C
600 °F
Descriptive Properties Value Comments
Saponification number 11.8