ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22

Category Fluid , Lubricant , Polyalphaolefin (PAO)
Manufacturer ConocoPhillips
Trade Name Syncon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommended for use in applications where operating conditions may be unfavorable or too severe for conventional mineral oilbased hydraulic oils. Syncon AW Hydraulic Fluid is formulated with synthetic polyalphaolefin (PAO) base oils and an ashless (zinc-free) additive package to provide excellent performance over a wide temperature range. It provides excellent wear protection for hydraulic pumps and motors, and protects hydraulic system components against rust and corrosion. It has outstanding oxidation resistance and thermal stability at high temperatures to minimize deposit formation and provide long service life. It also has excellent low-temperature properties for cold start-ups. It has excellent water-separating properties to minimize the formation of emulsions, and is resistant to excessive foaming that can cause poor or sluggish hydraulic system response. It has a high dielectric strength for use as insulating oil in electrical service bucket trucks. Syncon AW Hydraulic Fluid meets the performance requirements of all major hydraulic pump manufacturers, and is recommended for use in all types of high-pressure, high-speed hydraulic pumps.Applications: Industrial and mobile equipment operating under extreme temperature conditions Automated machine tools Bucket trucks (cherry pickers) used for servicing electrical power lines or for tree trimming Hydraulic hoists and service station lifts Mobile construction equipment Chain drives Electric motor bearingsSyncon AW Hydraulic Fluid meets the requirements of the following industry specifications:ANSI/AGMA Standard 9005-E02 Open Gear Lube meets the requirements of the following industry specification: DIN 51524 Part 2, Antiwear Hydraulic Oils, Type HLP ISO 11158:1997, Family H (Hydraulic Systems), Type HM U.S. Steel 127Features/Benefits: Outstanding oxidation resistance and thermal stability at high temperatures Outstanding pumpability at low temperatures Excellent wear protection for hydraulic pumps and motors Protects against rust and corrosion Separates rapidly from water Good foam resistance High dielectric strength Compatible with conventional mineral oils and commonly used sealsInformation provided by ConocoPhillips.
Physical Properties Metric English Comments
Specific Gravity 0.821 g/cc
0.821 g/cc
Density 0.820 g/cc
0.0296 lb/in³
Viscosity Measurement 127
127
Viscosity Index
Saybolt Viscosity at 100°F 115 SUS
115 SUS
Saybolt Viscosity at 210°F 42 SUS
42 SUS
Kinematic Viscosity at 40°C (104°F) 22 cSt
22 cSt
Kinematic Viscosity at 100°C (212°F) 4.6 cSt
4.6 cSt
Oxidative Stability 40 hour
40 hour
RPVOT; ASTM D2272
ASTM Color 0.50
0.50
ASTM D1500
Thermal Properties Metric English Comments
Pour Point -66.1 °C
-87.0 °F
Flash Point 218 °C
424 °F
Electrical Properties Metric English Comments
Dielectric Strength 35.0 kV/mm
889 kV/in
No thickness given
Chemical Properties Metric English Comments
Total Acid Number 0.17
0.17
[mg KOH/g]; ASTM D974
Descriptive Properties Value Comments
Copper Corrosion 1A
ASTM D130
Demulsibility 10 minutes to pass
ASTM D1401
FZG Scuffing Test 11 Failure Load Stage
ASTM D5182