ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1

Category Fluid , Lubricant , Urea Gellant
Manufacturer ConocoPhillips
Trade Name Tacna®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Tacna® EP Polyurea Grease NLGI Grade 1.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Tacna EP Polyurea Grease is a shear-stable product with exceptional extreme-pressure characteristics and excellent water resistance. It is recommended for use in steel mills, off-road equipment, fleet and commercial applications. It has excellent mobility at low temperatures. Applications Include:Fleet/Off-Road Equipment:Universal jointsHeavy-duty truck wheel bearingsWater pumpsIdler pulleysIndustrial Applications:Roller bearing requiring EP grease (temperatures up to 350°F (177°C))Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 1251 SUS
1251 SUS
Base Oil Property
Saybolt Viscosity at 210°F 94 SUS
94 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 235 cSt
235 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 18 cSt
18 cSt
Base Oil
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 66
66
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Four Ball Wear 0.450 mm
0.0177 in
Wear Scar
Penetration P(60), 1/10 mm 332
332
Timken Test 24900 g
55.0 lb
Thermal Properties Metric English Comments
Dropping Point 270 °C
518 °F
Descriptive Properties Value Comments
Color Green
Rust Test Pass