ConocoPhillips Tacna® Rx NLGI No. 2

Category Fluid , Lubricant , Lithium Gellant , Organic Soap Gellant
Manufacturer ConocoPhillips
Trade Name Tacna®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Tacna® Rx NLGI No. 2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motorcycles, on- and off-road trucks, buses, vans and construction equipment. It also is suited for industrial applications such as the heavily loaded antifriction and plain bearings found in gear boxes and electric motors commonly used in steel and aluminum manufacturing plants, as well as in mining equipment that requires a water-resistant, high-temperature grease. It is dyed red for easy identification and leak detection. Certified for use wherever NLGI GC-LB quality grease is recommended.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Viscosity Measurement 93
93
Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 795 SUS
795 SUS
Base Oil Property
Saybolt Viscosity at 210°F 77 SUS
77 SUS
Base Oil Property
Kinematic Viscosity at 40°C (104°F) 151 cSt
151 cSt
Base Oil
Kinematic Viscosity at 100°C (212°F) 14.4 cSt
14.4 cSt
Base Oil
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 40
40
Four Ball Extreme Pressure, Weld Load 400 kg
882 lb (mass)
Four Ball Wear 0.430 mm
0.0169 in
Penetration P(60), 1/10 mm 280
280
Timken Test 24900 g
55.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -23.3 °C
-10.0 °F
Dropping Point 260 °C
500 °F
Descriptive Properties Value Comments
ASTM Rust Test (A & B) Pass
Color Red
Low Temperature Mobility 0.2 gm/sec
at 0°F
0.4 gm/sec
at 10°F
0.8 gm/sec
at 20°F
Oil Separation 0.5 wt.%
Oxidation Resistance 16 psi drop/500 hrs
29 psi drop/1000 hrs
3 psi drop/100 hrs
Soap Type (Thickener) Lithium Complex
Water Washout 0.02
100°F
0.04
175°F
Wheel Bearing Leakage 5 wt.%
212°F