Material Notes:
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
ISO 2577
Melt Flow >= 50 g/10 min

@Load 10.0 kg,
Temperature 240 °C
>= 50 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 36.0 MPa
5220 psi
ISO 527
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527
Elongation at Break >= 60 %
>= 60 %
ISO 527
Tensile Modulus 2.00 GPa
290 ksi
ISO 527
Flexural Modulus 1.90 GPa
276 ksi
ISO 178
Izod Impact, Notched 0.600 J/cm

@Temperature 23.0 °C
1.12 ft-lb/in

@Temperature 73.4 °F
ISO 180/A
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C

@Load 5.00 kg
253 °F

@Load 11.0 lb
50°C/hr; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in