Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cossa Polimeri ESTAPROP HK 4000 CH-HT Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Cossa Polimeri S.r.L.
Trade Name ESTAPROP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cossa Polimeri ESTAPROP HK 4000 CH-HT Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polypropylene copolymer, high fluidityInformation provided by Cossa Polimeri S.r.l.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ASTM D 955
Melt Flow 55 g/10 min

@Load 2.16 kg,
Temperature 230 °C
55 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Flexural Modulus 1.30 GPa
189 ksi
ASTM D 790
Izod Impact, Notched 0.450 J/cm

@Temperature 23.0 °C
0.843 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C

@Load 5.10 kg
185 °F

@Load 11.2 lb
50°C/hr; ASTM D 1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in