Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure

Category Polymer , Thermoset , Epoxy
Manufacturer Cotronics
Trade Name Bond-It™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms high strength bonds to difficult metals, plastics, glass, ceramics, composites, etc. Cures at room temperature with high temperature strength and good electrical and thermal shock resistance. Good chemical resistance.Applications: bonding ceramic wear tips to aluminum, brake pads to metal, assembling and repairing machines, aerospace and automotive applications, etc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Moisture Absorption at Equilibrium 0.80 %
0.80 %
Viscosity 5000 cP
5000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Tensile Strength, Ultimate 34.5 MPa
5000 psi
Elongation at Break 3.0 %
3.0 %
Thermal Properties Metric English Comments
CTE, linear 62.0 µm/m-°C

@Temperature 20.0 °C
34.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.01 W/m-K
7.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
400 °F
Shrinkage 1.0 %
1.0 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
Dielectric Strength 19.7 kV/mm
500 kV/in
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 121 °C
0.250 hour

@Temperature 250 °F