Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant

Category Polymer , Thermoset , Epoxy
Manufacturer Cotronics
Trade Name Duralco™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Duralco™ 4460 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent adhesion to metals, plastics, ceramics and glass. High bond strength, low moisture absorption, high thermal stability, low shrinkage and excellent chemical, electrical, and radiation resistance.Applications: Ideal for ultra thin bond lines, sealing porous materials and protecting boding and coating critical electronic components, strain gauges, etc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
Moisture Absorption at Equilibrium 0.10 %
0.10 %
Viscosity 600 cP
600 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Tensile Strength, Ultimate 71.0 MPa
10300 psi
Elongation at Break 5.0 %
5.0 %
Thermal Properties Metric English Comments
CTE, linear 64.0 µm/m-°C

@Temperature 20.0 °C
35.6 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.576 W/m-K
4.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 316 °C
600 °F
Shrinkage 0.50 %
0.50 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Strength 19.7 kV/mm
500 kV/in
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 121 °C
4.00 hour

@Temperature 250 °F