Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Cotronics Duralco™ 4540 Machinable Epoxy

Category Polymer , Thermoset , Epoxy
Manufacturer Cotronics
Trade Name Duralco™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Duralco™ 4540 Machinable Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Patches, fills, seals, and repairs with outstanding adhesion, ductility, thermal conductivity and shock resistance.Corrosion Resistance: excellent resistance to chemicals and solventsApplications: repairing leaks, solder joints, cracks, holes, castings, heating elements, cooling coils, high temperature instruments, assemblies.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Moisture Absorption at Equilibrium 0.20 %
0.20 %
Viscosity 30000 cP
30000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Tensile Strength, Ultimate 68.9 MPa
10000 psi
Elongation at Break 1.2 %
1.2 %
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 5.04 W/m-K
35.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
500 °F
Shrinkage 0.10 %
0.10 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+8 ohm-cm
1.00e+8 ohm-cm
Dielectric Strength 3.94 kV/mm
100 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 121 °C
1.00 hour

@Temperature 250 °F
Copyright © lookpolymers.com All Rights Reserved