High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracked composites, dies, fixtures, jigs, etc. Electrically non-conductive.Corrosion Resistance: resistant to most chemicals, solvents, acids and bases.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Moisture Absorption at Equilibrium 0.15 %
0.15 %
Viscosity 50000 cP
50000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 95
95
Tensile Strength, Ultimate 81.4 MPa
11800 psi
Elongation at Break 2.0 %
2.0 %
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 2.59 W/m-K
18.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 371 °C
700 °F
Shrinkage 0.10 %
0.10 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
Dielectric Strength 17.7 kV/mm
450 kV/in
Processing Properties Metric English Comments
Cure Time 240 - 360 min

@Temperature 121 °C
4.00 - 6.00 hour

@Temperature 250 °F
Users viewing this material also viewed the following: