Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base

Category Ceramic
Manufacturer Cotronics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Single component system with a paint consistency.
Mechanical Properties Metric English Comments
Flexural Strength 4.14 MPa
600 psi
Compressive Strength 8.27 MPa
1200 psi
Thermal Properties Metric English Comments
CTE, linear 7.20 µm/m-°C

@Temperature 20.0 °C
4.00 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.288 W/m-K
2.00 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1430 °C
2600 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Dielectric Strength 7.87 kV/mm
200 kV/in