Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Covestro
Trade Name Bayflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayflex® 180 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption at Saturation 0.20 %
0.20 %
240 hours; Bayer Test
Linear Mold Shrinkage 0.017 cm/cm
0.017 in/in
Bayer Test
Mechanical Properties Metric English Comments
Hardness, Shore D 69
69
ASTM D2240
Tensile Strength, Ultimate 28.0 MPa
4060 psi
ASTM D638/D412
Elongation at Break 125 %
125 %
ASTM D638/D412
Flexural Modulus 0.590 GPa
85.6 ksi
ASTM D790
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Tear Strength 105 kN/m
599 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
CTE, linear 153 µm/m-°C

@Temperature 20.0 °C
85.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696