Covestro Desmopan® 385 Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® 385 Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Desmopan 385 is a TPU on the basis of a standard ester.Applications: Screen sections, films, hoses, seals, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
DIN 53505
Elongation at Break >= 50 %
>= 50 %
Nominal
Compression Set 30 %
30 %
70 hr; 22°C
55 %

@Temperature 70.0 °C
55 %

@Temperature 158 °F
24 hr
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 150 µm/m-°C

@Temperature 20.0 °C
83.3 µin/in-°F

@Temperature 68.0 °F
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 8.00e+11 ohm-cm
8.00e+11 ohm-cm
Surface Resistance 5.00e+11 ohm
5.00e+11 ohm
Dielectric Constant 5.6

@Frequency 1e+6 Hz
5.6

@Frequency 1e+6 Hz
6.5

@Frequency 100 Hz
6.5

@Frequency 100 Hz
Dielectric Strength 17.5 kV/mm
445 kV/in
Dissipation Factor 0.029

@Frequency 100 Hz
0.029

@Frequency 100 Hz
0.060

@Frequency 1e+6 Hz
0.060

@Frequency 1e+6 Hz