Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Desmopan® 445 Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® 445 Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding gradegrease and oil-resistantgood heat resistancelow compression setApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
3s; ISO 868
Hardness, Shore D 44
44
15s; ISO 868
Tensile Strength at Break 38.0 MPa
5510 psi
ISO 527-1/-2
Tensile Strength, Yield 38.0 MPa
5510 psi
parallel; ISO 527-3
8.00 MPa

@Strain 100 %
1160 psi

@Strain 100 %
ISO 527-1/-2
20.0 MPa

@Strain 300 %
2900 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 25
25
mm³; ISO 4649
Compression Set 35 %

@Temperature 70.0 °C
35 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
North America
South and Central America
Feature Release agent
Form Pellets
Process Injection Molding
Users viewing this material also viewed the following: