injection molding gradevery good hydrolysis and microbial resistancehigh mechanical strengthgood low-temperature flexibilityApplicationToysTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
3s; ISO 868
Hardness, Shore D 33
33
15s; ISO 868
Tensile Strength at Break 43.0 MPa
6240 psi
ISO 527-1/-2
Tensile Strength, Yield 43.0 MPa
6240 psi
parallel; ISO 527-3
7.00 MPa

@Strain 100 %
1020 psi

@Strain 100 %
ISO 527-1/-2
14.0 MPa

@Strain 300 %
2030 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 40
40
mm³; ISO 4649
Compression Set 30 %

@Temperature 23.0 °C
30 %

@Temperature 73.4 °F
ISO 815
65 %

@Temperature 70.0 °C
65 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Feature Release agent
Form Pellets
Process Injection Molding