Covestro Desmopan® DP 3065D Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 3065D Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding gradehigh mechanical strengthexcellent abrasion resistancegood wear resistancevery short cycle timesApplicationTechnical partsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
3s; ISO 868
Hardness, Shore D 65
65
15s; ISO 868
Tensile Strength at Break 60.0 MPa
8700 psi
ISO 527-1/-2
Tensile Strength, Yield 60.0 MPa
8700 psi
parallel; ISO 527-3
26.0 MPa

@Strain 100 %
3770 psi

@Strain 100 %
ISO 527-1/-2
45.0 MPa

@Strain 300 %
6530 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 18
18
mm³; ISO 4649
Compression Set 26 %

@Temperature 23.0 °C
26 %

@Temperature 73.4 °F
ISO 815
38 %

@Temperature 70.0 °C
38 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America