Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Desmopan® DP 3070AU Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Covestro
Trade Name Desmopan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Desmopan® DP 3070AU Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
injection molding gradefree from plasticizersApplicationInjection molded engineering partshard - soft systemsAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
3s; ISO 868
Tensile Strength at Break 25.0 MPa
3630 psi
ISO 527-1/-2
Tensile Strength, Yield 25.0 MPa
3630 psi
parallel; ISO 527-3
2.50 MPa

@Strain 100 %
363 psi

@Strain 100 %
ISO 527-1/-2
4.60 MPa

@Strain 300 %
667 psi

@Strain 300 %
ISO 527-1/-2
Elongation at Break >= 300 %
>= 300 %
ISO 527-1/-2
Abrasion 50
50
mm³; ISO 4649
Compression Set 24 %

@Temperature 23.0 °C
24 %

@Temperature 73.4 °F
ISO 815
52 %

@Temperature 70.0 °C
52 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved