Material Notes:
As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
3s; ISO 868
Hardness, Shore D 75
75
15s; ISO 868
Tensile Strength at Break 34.0 MPa
4930 psi
ISO 527-1/-2
Tensile Strength, Yield 34.0 MPa
4930 psi
parallel; ISO 527-3
30.0 MPa

@Strain 100 %
4350 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break 300 %
300 %
ISO 527-1/-2
Abrasion 44
44
mm³; ISO 4649
Compression Set 45 %

@Temperature 23.0 °C
45 %

@Temperature 73.4 °F
ISO 815
49 %

@Temperature 70.0 °C
49 %

@Temperature 158 °F
ISO 815
Descriptive Properties Value Comments