Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding (Melt Temperature: 495-530°F, Mold Temperature: 195-250°F)Petlon® is manufactured by Albis Plastics Corporation and is a registered trademark of Bayer Corporation.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Physical Properties Metric English Comments
Density 1.66 g/cc
0.0600 lb/in³
ASTM D792
Water Absorption 0.040 %
0.040 %
(24 hr); ASTM D570
Moisture Absorption at Equilibrium 0.13 %
0.13 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86
86
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength at Break 148.9 MPa
21600 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 222 MPa
32200 psi
ASTM D790
Flexural Modulus 10.69 GPa
1550 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 150 °C
302 °F
RTI
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648
Vicat Softening Point >= 225 °C
>= 437 °F
ASTM D1525
UL RTI, Mechanical without Impact 150 °C
302 °F
Flammability, UL94 V-0
V-0
0.028 in
Electrical Properties Metric English Comments
Dielectric Constant 3.7

@Frequency 60 Hz
3.7

@Frequency 60 Hz
ASTM D150
Dielectric Strength 22.7 kV/mm
577 kV/in
ASTM D149
Arc Resistance 111 sec
111 sec
ASTM D495
Comparative Tracking Index 220 V
220 V
ASTM D3638
Processing Properties Metric English Comments
Melt Temperature 257 - 277 °C
495 - 531 °F
Injection
Mold Temperature 91.0 - 121 °C
196 - 250 °F