Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Petlon® PC/PET 36A 620UV Yellow Semi-Crystalline PET, 10% Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/PET Polyester Blend , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Petlon® PC/PET 36A 620UV Yellow Semi-Crystalline PET, 10% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: Good Thermal and Dimensional Stability, Good Chemical ResistanceApplications: Automotive Panels, Electronic Housings, Pump HousingsProcessing: Injection Molding (Melt Temperature: 500-530°F, Mold Temperature: 165-200°F)Petlon® is manufactured by Albis Plastics Corporation and is a registered trademark of Bayer Corporation.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
(24 hr); ASTM D570
Moisture Absorption at Equilibrium 0.24 %
0.24 %
ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0060 cm/cm
0.0010 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength at Break 62.1 MPa
9010 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Yield Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 3.86 GPa
560 ksi
ASTM D790
Izod Impact, Notched 1.39 J/cm
2.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 26.0 µm/m-°C

@Temperature 20.0 °C
14.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 114 °C
237 °F
ASTM D648
Flammability, UL94 HB
HB
0.059 in; Albis Internal test
Electrical Properties Metric English Comments
Dielectric Constant 3.2
3.2
Dielectric Strength >= 27.6 kV/mm
>= 701 kV/in
ASTM D149
Processing Properties Metric English Comments
Melt Temperature 260 - 277 °C
500 - 531 °F
Injection
Mold Temperature 74.0 - 93.0 °C
165 - 199 °F
Copyright © lookpolymers.com All Rights Reserved