Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa

@Strain 50.0 %
2760 psi

@Strain 50.0 %
Elongation at Break >= 50 %
>= 50 %
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 181 µm/m-°C

@Temperature 20.0 °C
101 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C
140 °F
Vicat Softening Point 190 °C
374 °F
50°C/h 50N
Glass Transition Temp, Tg -15.0 °C
5.00 °F
10°C/min
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL Recognized
Processing Properties Metric English Comments
Melt Temperature 210 °C
410 °F
Injection Molding
Mold Temperature 30.0 °C
86.0 °F
Injection Molding
Injection Pressure 45.0 MPa
6530 psi